Plastic crates will fade due to many factors. The fading of the plastic turnover box is related to the light resistance, oxygen resistance, heat resistance, acid and alkali resistance of the colorant and the characteristics of the resin used.
The following is a detailed analysis of the coloring and fading factors of the plastic turnover box:
1. Lightfastness of the colorant
The light fastness of the colorant directly affects the fading of the product. For outdoor products exposed to strong light, the light fastness (light fastness) level requirement of the colorant used is an important indicator. The light fastness level is poor, and the turnover box will quickly fade during use. The light resistance grade selected for weather-resistant products should not be lower than six grades, preferably seven or eight grades, and indoor products can choose four or five grades.
The light resistance of the carrier resin also has a great influence on the color change, and the molecular structure of the resin changes and fades after being irradiated by ultraviolet rays. Adding light stabilizers such as ultraviolet absorbers to the masterbatch can improve the light resistance of colorants and colored plastic products.
2. Heat resistance
The thermal stability of a heat-resistant pigment refers to the degree of thermal weight loss, discoloration, and fading of the pigment at the processing temperature.
Inorganic pigments are composed of metal oxides and salts, with good thermal stability and high heat resistance. The pigments of organic compounds will undergo molecular structure changes and a small amount of decomposition at a certain temperature. Especially for PP, PA, PET products, the processing temperature is above 280℃. When selecting colorants, one should pay attention to the heat resistance of the pigment, and the heat resistance time of the pigment should be considered on the other hand. The heat resistance time is usually 4-10min. .
3. Antioxidant
Some organic pigments undergo macromolecular degradation or other changes after oxidation and gradually fade. This process is high temperature oxidation during processing, and oxidation when encountering strong oxidants (such as chromate in chrome yellow). After the lake, azo pigment and chrome yellow are mixed, the red color will gradually fade.
4. Acid and alkali resistance
The fading of the plastic turnover box is related to the chemical resistance of the colorant (acid and alkali resistance, oxidation-reduction resistance). For example, molybdenum chrome red is resistant to dilute acid, but is sensitive to alkalis, and cadmium yellow is not acid resistant. These two pigments and phenolic resins have a strong reducing effect on certain colorants, which seriously affect the heat resistance and weather resistance of the colorants and cause fading.
In view of the fading of the plastic turnover box, it should be selected after comprehensive evaluation of the above-mentioned properties of the required pigments, dyes, surfactants, dispersants, carrier resins and anti-aging additives according to processing conditions and use requirements.
*Dongguan Jiehua Plastic Products Co., Ltd. was established in 2001. It is an enterprise specializing in the production, sales and research and development of plastic products (plastic pallets, plastic boxes, plastic baskets, hollow board boxes, etc.) and anti-static products. The company has a professional technical team composed of dozens of senior mold engineers, structural designers, and a dozen mechanical engineers and quality engineers, and a high-quality professional management and marketing team. Its business outlets are all over the Pearl River Delta, and in Shanghai, There are sales companies in Zhejiang and other places, with a large transportation team, and strive to provide customers with better services. Welcome to call! Jiehua Plastic Alibaba Store: https://ajiehua.1688.com/
Solid-state Capacitors / Motor Starting Capacitors
Solid - state capacitors are all called: solid - state Aluminum Electrolytic Capacitors.It with the ordinary capacitance (that is, the liquid aluminum electrolytic capacitors) the biggest difference is that use different dielectric material, liquid aluminum capacitor dielectric material as the electrolyte, and solid-state capacitor dielectric material is conductive polymer materials.Solid-state capacitors / Motor starting capacitors
Solid-state capacitors,Motor starting capacitors,Solid-State Capacitors,Solid-State Small Size Capacitors,Solid-State Low Impedance Capacitors,Long Life Solid-State Capacitors
YANGZHOU POSITIONING TECH CO., LTD. , https://www.pst-thyristor.com